Brand Name: | Tuwe |
Model Number: | TW-90FBY |
MOQ: | 1000kg |
Price: | USD 650-990/TON |
Packaging Details: | 25kg/500kg-1000kg/Jumbo bag |
Payment Terms: | T/T |
90℃ Anti-Termite And Rat-Resistant Polyvinyl Chloride Sheath Compound Complying With IEC Standards, Anti-Rat Pvc Particles
The recommended temperature settings for each zone of the extruder are as follows:
Location | Zone 1 | Zone 2 | Zone 3 | Zone 4 | Machine neck | Machine head | Mould port |
Temperature/°C | 150 | 155 | 160 | 170 | 175 | 175 | 170 |
The best extrusion temperature depends on the specific structure of the screw, such as aspect ratio, compression ratio, etc. If you have any technical problems after purchasing PVC sheath materials, please contact us and we will arrange engineers to provide solutions. TUWEI is committed to providing one-stop services for PVC processing, production, formulation and technology.
N0. | Items | Unit | Results of Testing | Test Method | |
1 | Color | / |
Difference from standard color plate ≤ Δ1.0 |
||
2 | Granule size for square particles |
mm
|
3-5mm | ||
3 | Density | g/cm3 | 1.3-1.65(Customizable) | ||
4 | Tensile Strength | MPa | 20.5 | GB1040 | IEC60811-1-1 |
5 | Elongation at Break | % | 320 | ||
6 | Thermal Deformation | % | 30 | GB/T8815 | |
7 | Brittle Temperature | °C | -20°C tested | GB5470 | IEC60811-1-4 |
8 | Thermal stability time at 200℃ | min | 100 | GB/T8815 | |
9 | Volume resistivity at 20℃ | Ω·m | 8x1010 | GB1410 | IEC60167 |
10 | Dielectric Strength | MV/m | 25 | GB1408 | IEC60243 |
11 | Thermal aging strength | ℃xday | 100x10 | GB/T2951 | |
12 | Tensile strength after aging | MPa | 19.8 | ||
13 | Change rate of tensile strength | % | -3.4 | ||
14 | Elongation at break after aging | % | 200 | ||
15 | Change rate of elongation at break | % | -3.4 | ||
16 | Quality loss due to thermal aging | g/cm3 | 8 | ||
17 | termite prevention performance |
Our PVC Compound Granules are perfect for a wide range of applications and scenarios, including:
Our PVC Compound Granules are designed to meet the specific needs of our customers, and we take pride in providing top-quality products and technical support. Our highly skilled technical team is available to assist with any questions or concerns regarding the use of our PVC Compound Granules. We offer a range of services, including:
We are committed to delivering exceptional customer service and ensuring the success of our customers. Contact us to learn more about how our PVC Compound Granules can meet your specific needs.
Brand Name: | Tuwe |
Model Number: | TW-90FBY |
MOQ: | 1000kg |
Price: | USD 650-990/TON |
Packaging Details: | 25kg/500kg-1000kg/Jumbo bag |
Payment Terms: | T/T |
90℃ Anti-Termite And Rat-Resistant Polyvinyl Chloride Sheath Compound Complying With IEC Standards, Anti-Rat Pvc Particles
The recommended temperature settings for each zone of the extruder are as follows:
Location | Zone 1 | Zone 2 | Zone 3 | Zone 4 | Machine neck | Machine head | Mould port |
Temperature/°C | 150 | 155 | 160 | 170 | 175 | 175 | 170 |
The best extrusion temperature depends on the specific structure of the screw, such as aspect ratio, compression ratio, etc. If you have any technical problems after purchasing PVC sheath materials, please contact us and we will arrange engineers to provide solutions. TUWEI is committed to providing one-stop services for PVC processing, production, formulation and technology.
N0. | Items | Unit | Results of Testing | Test Method | |
1 | Color | / |
Difference from standard color plate ≤ Δ1.0 |
||
2 | Granule size for square particles |
mm
|
3-5mm | ||
3 | Density | g/cm3 | 1.3-1.65(Customizable) | ||
4 | Tensile Strength | MPa | 20.5 | GB1040 | IEC60811-1-1 |
5 | Elongation at Break | % | 320 | ||
6 | Thermal Deformation | % | 30 | GB/T8815 | |
7 | Brittle Temperature | °C | -20°C tested | GB5470 | IEC60811-1-4 |
8 | Thermal stability time at 200℃ | min | 100 | GB/T8815 | |
9 | Volume resistivity at 20℃ | Ω·m | 8x1010 | GB1410 | IEC60167 |
10 | Dielectric Strength | MV/m | 25 | GB1408 | IEC60243 |
11 | Thermal aging strength | ℃xday | 100x10 | GB/T2951 | |
12 | Tensile strength after aging | MPa | 19.8 | ||
13 | Change rate of tensile strength | % | -3.4 | ||
14 | Elongation at break after aging | % | 200 | ||
15 | Change rate of elongation at break | % | -3.4 | ||
16 | Quality loss due to thermal aging | g/cm3 | 8 | ||
17 | termite prevention performance |
Our PVC Compound Granules are perfect for a wide range of applications and scenarios, including:
Our PVC Compound Granules are designed to meet the specific needs of our customers, and we take pride in providing top-quality products and technical support. Our highly skilled technical team is available to assist with any questions or concerns regarding the use of our PVC Compound Granules. We offer a range of services, including:
We are committed to delivering exceptional customer service and ensuring the success of our customers. Contact us to learn more about how our PVC Compound Granules can meet your specific needs.